Procedure
- Begin heating water to 80° C and add Phase A ingredients one by one, mixing each until uniform.
- Combine Phase B ingredients, and heat to 80 – 85° C until melted.
- Add Phase B to Phase A under agitation and mix at high speed until emulsion is uniform.
- Check pH and adjust to 4-5 as necessary.
- Cool to 45° C or under and pour into containers.
Stability Information
Three months at 50° C, three months at room temperature, three freeze/thaw cycles.
Supplier Information
- Koster Keunen, Inc.
- Barentz
- DuPont
- Nouryon
- Lincoln Manufacturing
Ingredient Trade Name |
INCI Name |
% |
|---|---|---|
| Phase A | ||
| Deionized Water | Aqua | 83.2 |
| Jaguar C-172 | Guar Hydroxypropyltrimonium Chloride | 0.4 |
| Zemea Propanediol3 | Propanediol | 2.0 |
| Celquat SC-2304 | Polyquaternium-10 | 0.2 |
| Lincoserve WpH-LO5 | Pentylene Glycol, Propanediol, Caprylyl Glycol, Ethylhexylglycerin | 1.0 |
| Citric Acid | Citric Acid | 0.2 |
| Phase B | ||
| Kostol TMC-25 | Cetearyl Alcohol (and) Behentrimonium Chloride | 6.0 |
| Synkos M-1063 | Synthetic Wax | 5.0 |
| Kester Wax K-24 | Lauryl Laurate | 2.0 |