Procedure
Begin heating water to 80℃ and add Phase A ingredients one at a time, mixing until uniform. Heat Phase B to about 80-85℃. Add Phase B to Phase A and mix at high speed until emulsion is smooth. Cool slowly at lower speed to 55-60℃. Add Phase C ingredients, one at a time mixing after each addition. Pump into containers.
Stability
Three months at 45℃, three months at room temperature, three freeze/thaw cycles.
Suppliers
- Koster Keunen, Inc.
- Brenntag Specialties
- Angus
- BASF
Ingredient Trade Name |
INCI Name |
% |
---|---|---|
Phase A | ||
Deionized Water | Aqua | 50.95 |
980 Carbomer2 | Carbomer | 0.05 |
AMP 953 | Aminomethyl Propanol | 0.5 |
Propylene Glycol | Propylene Glycol | 5.0 |
Luviskol VA 644 | VP/VA Copolymer | 3.5 |
Aquaflex XL-302 | Polyimide-1 | 5.0 |
Phase B | ||
Kester Wax SWR1 | C20-40 Alcohols, Candelilla Wax, Carnauba Wax, Glycol Distearate, Montan Acid Wax | 10.0 |
Kester Wax CT1 | C32-36 Isoalkyl Stearate, Polyhydroxystearic Acid, Stearyl Behenate, Cetearyl Alcohol, Polyglyceryl-3 Stearate, Polysorbate 60 | 10.0 |
Kostol PGP1 | Polyglyceril-3 Stearate, Beheneth-5 | 2.0 |
Stearic Acid | Stearic Acid | 2.0 |
Phase C | ||
SD Alcohol | Alcohol Denatured | 10.0 |
Optiphen2 | Phenoxyethanol, Caprylyl Glycol | 1.0 |